Solutions For Cracked Titanium Plates

Jan 12, 2024

Cracking is often a defect in titanium plate welding. Titanium weld cracks are cold cracks and are mainly caused by hydrogen in the weld. The sources of hydrogen mainly include moisture and oil in the plate and wire, and environmental humidity is the main cause of hydrogenation in the weld.

There is a large amount of hydrogen dissolved in the molten pool under the action of high temperature during welding. During the cooling and solidification of the weld, hydrogen escapes rapidly due to the rapid decrease in solubility. If the weld cools too quickly, hydrogen will not escape and remain in the weld, and the weld will be supersaturated with hydrogen, which will diffuse as far as possible, contributing to further embrittlement of the region.

Titanium Plate/SheetGr4 Pure Titanium PlateGr 2 Titanium Plate

 

 

If the notch effect is present at this location and the hydrogen concentration is high enough, cracking may occur. Especially during winter construction, when ambient temperatures are low, water vapor adheres to the titanium plate, creating conditions for hydrogenation of the weld. Due to the thinness of the titanium plate (1.2 mm), the plate is relatively "eaten away" and the temperature rises slowly. The corresponding titanium composite layer weld cooling rate is too fast. During the cooling process, the residual hydrogen in the weld does not have time to escape. The presence of oversaturation in the weld eventually leads to the appearance of cracks.

Therefore, during the welding process of titanium steel composite plate, the surface of the base metal and welding wire must be carefully cleaned, and the ambient temperature must be maintained at a temperature of not less than 5℃. In winter construction, use the flame to preheat the surface of the base steel, one is to remove the moisture around the weld; the second is to increase the temperature of the weldment and reduce the cooling rate of the weld.