How To Weld Titanium Tubing?

Jan 12, 2024

Titanium Pipe Welding Technical Information: Titanium pipe welding is a TiG welding process that uses pilot gas to effectively protect the weld zone. Because titanium has special physical and chemical properties, its welding process is very different from other metals. Titanium pipe welding must ensure that: (1) 250 ℃ above the weld zone metal is not affected by the reaction gas N, 0, H and harmful impurity elements C, Fe, Mn, etc.. (2) Can not form a coarse crystal structure. (3) Can not produce large welding residual stress and residual deformation. Therefore, the welding process must be in accordance with the pre-determined construction sequence, in strict accordance with the process quality management standards, the implementation of the whole process of quality control. People, machines, materials, methods and other factors are in a good controlled state, so as to ensure the welding quality of titanium tubes in a reasonable time.

Titanium pipe and accessories: there should be manufacturers of factory certificates and quality certificates. Its specifications, chemical composition, mechanical properties and supply conditions review should be in line with DIN17850 standard requirements.

Titanium pipe welding materials

Ti-6al-4v Gr5 Grade5 Titanium Alloy TubingTitanium Tubing For Bicycle ManufacturingTitanium Capillary Tube

 

 

Welding wire; welding wire number ERTi-2, select the wire should meet the following requirements:

(l) The chemical composition and mechanical properties of the welding wire should be equivalent to the base material;

(2) If the weldment requires higher plasticity, a higher purity wire than the base metal should be used.

Argon: purity of not less than 99.98%, water content of less than 50 Mg/m3 of industrial-grade pure argon.

Before using argon, you should check the factory certificate on the bottle to verify the purity of argon. Then check whether the bottle valve is leaking or malfunctioning. The titanium tube welding process adopts manual tungsten inert gas shielded welding (GTAW) welding method in the atmosphere. After welding, the internal and external surfaces within 25mm of the bevel of the titanium tube and all sides of the titanium tube are cleared of oil and dirt, and then painted with an austenitic stainless steel wire brush. Mechanical methods such as reamer to remove oxide film, burrs and surface defects. Cleaning tools should be dedicated and kept clean; mechanically cleaned bevel and filler wire surface should be degreased with sulfur-free acetone or ethanol before use. During the welding process, special protective measures are used to make the temperature of the titanium tube welding area exceed 400℃, and some or all of them are effectively protected by argon gas to achieve the purpose of titanium tube welding.

Construction Preparation → Material Acceptance → Line Inspection → Cutting Bevel Processing → Peripheral Processing → Welding Pair → Welding Seam → Visual Inspection of Welding Seam → Welding Seam PT, RT Inspection → Prefabricated Section Hydrostatic Test → Drainage, Drying → Pipeline Confinement and Transportation → On-site Assembly.